Correction to Creating Water Vapor Barrier Coatings from Hydrophilic

Jan 10, 2014 - Correction to Creating Water Vapor Barrier Coatings from Hydrophilic Components. Gerald Findenig, Simon Leimgruber, Rupert Kargl*, Stef...
0 downloads 0 Views 99KB Size
Addition/Correction www.acsami.org

Correction to Creating Water Vapor Barrier Coatings from Hydrophilic Components Gerald Findenig, Simon Leimgruber, Rupert Kargl,* Stefan Spirk, Karin Stana-Kleinschek, and Volker Ribitsch ACS Appl. Mater. Interfaces 2012, 4 (6), 3199−3206; 10.1021/am300542h All water vapor transmission rate (WVTR) values in this publication refer to a substrate size of 0.25 m2 instead of 1 m2. The WVTR unit in this publication should therefore be g 0.25 m−2 day−1. The authors apologize for this calculation error.

Published: January 10, 2014 © 2014 American Chemical Society

1337

dx.doi.org/10.1021/am405894a | ACS Appl. Mater. Interfaces 2014, 6, 1337−1337