Correction to Improved Synthesis of Graphene Oxide - American

Jan 5, 2018 - for the improved method, KMnO4 (18.0 g, 6 wt equiv) was slowly added in 6 equal portions to a 9:1 mixture of concentrated H2SO4/H3PO4 ...
0 downloads 0 Views 237KB Size
www.acsnano.org

Correction to Improved Synthesis of Graphene Oxide Daniela C. Marcano, Dmitry V. Kosynkin, Jacob M. Berlin, Alexander Sinitskii, Zhengzong Sun, Alexander S. Slesarev, Lawrence B. Alemany, Wei Lu, and James M. Tour* ACS Nano 2010, 4 (8), 4806−4814. DOI: 10.1021/nn1006368.

I

n the Experimental Procedures section, the order of addition of reagents in the description of the improved method is incorrect. The correct procedure is as follows: for the improved method, KMnO4 (18.0 g, 6 wt equiv) was slowly added in 6 equal portions to a 9:1 mixture of concentrated H2SO4/H3PO4 (360:40 mL) and graphite flakes (3.0 g, 1 wt equiv), producing a slight exotherm that should not exceed 35−40 °C. The reaction was then heated to 50 °C and stirred for 12 h. The reaction was cooled to room temperature and poured onto ice (400 mL) containing 30% H2O2 (3 mL). This correction is important because, in the instances where there would be different addition order, the KMnO4 might be in high concentration in the acid mixture, and this can become explosive.

Received: January 5, 2018

© XXXX American Chemical Society

A

DOI: 10.1021/acsnano.8b00128 ACS Nano XXXX, XXX, XXX−XXX

Additions and Corrections

Cite This: ACS Nano XXXX, XXX, XXX−XXX