Addition to “Degradation of the Polymeric Brominated Flame

Mar 27, 2019 - Addition to “Degradation of the Polymeric Brominated Flame Retardant 'Polymeric FR' by Heat and UV Exposure” ...
0 downloads 0 Views 291KB Size
This is an open access article published under an ACS AuthorChoice License, which permits copying and redistribution of the article or any adaptations for non-commercial purposes.

Addition/Correction Cite This: Environ. Sci. Technol. XXXX, XXX, XXX−XXX

pubs.acs.org/est

Addition to “Degradation of the Polymeric Brominated Flame Retardant ‘Polymeric FR’ by Heat and UV Exposure” Christoph Koch,* Milen Nachev, Julia Klein, Daniel Köster, Oliver J. Schmitz, Torsten C. Schmidt, and Bernd Sures Environ. Sci. Technol. 2019, 53 (3), 1453−1462. DOI: 10.1021/acs.est.8b03872 he authors wish to clarify that whereas the first author, Christoph Koch, is affiliated with Deutsche Rockwool GmbH & Co. KG, none of the funding for this project was provided by this company, nor has there been any other influence regarding this research project. The publication is part of his Ph.D. project, which he already started before he was affiliated with Deutsche Rockwool GmbH & Co. KG and which he continued in his free time. The study was solely supported by university funds. The Conflict of Interest statement and other funding sources are correct as published in this article.

Environ. Sci. Technol. Downloaded from pubs.acs.org by 146.185.205.153 on 03/30/19. For personal use only.

T

© 2019 American Chemical Society

A

DOI: 10.1021/acs.est.9b01145 Environ. Sci. Technol. XXXX, XXX, XXX−XXX