Correction to “Atomic Layer Deposition of Spinel Lithium Manganese Oxide by Film-Body-Controlled Lithium Incorporation for Thin-Film Lithium-Ion Batteries” Ville Miikkulainen,* Amund Ruud, Erik Østreng, Ola Nilsen, Mikko Laitinen, Timo Sajavaara, and Helmer Fjellvåg J. Phys. Chem. C 2014, 118 (2), 1258−1268. DOI: 10.1021/jp409399y

F

igure 2 in the original article was incorrectly reproduced, and it shows erroneous data points for “Growth per cycle/ Å” and “Li/(Li+Mn) in film” in the figure panel (a). The corrected figure is given here as Figure 1.

Figure 1. Growth per cycle and relative lithium composition for LixMnyOz films deposited with Li(thd) as the lithium precursor for films with (a) 4000 and (b) 1000 deposition cycles.