Correction to Zinc Blende and Wurtzite Crystal Phase Mixing and Transition in Indium Phosphide Nanowires Keitaro Ikejiri,* Yusuke Kitauchi, Katsuhiro Tomioka, Junichi Motohisa, and Takashi Fukui Nano Lett. 2011, 11, (10), 4314−4318. DOI: 10.1021/nl202365q. On page 4314 in the right-hand column lines 16−19, “Under the high Tg and low V/III ratio condition, we obtain ZB InP nanowires, whereas the crystal structure changes from ZB to WZ when Tg is decreased and V/III ratio is increased.” should be “Under the low Tg and high V/III ratio condition, we obtain ZB InP nanowires, whereas the crystal structure changes from ZB to WZ when Tg is increased and V/III ratio is decreased.”

On page 4315, the description in Figure 1, which reads “NW1: Tg = 660 °C, V/III = 18” and “NW3: Tg = 600 °C,V/ III = 55”, should be “NW1: Tg = 600 °C, V/III = 55” and “NW3: Tg = 660 °C, V/III = 18”. On page 4315 in the left-hand column lines 21−22, “...were 660 °C and 18, respectively. WZ nanowire (NW3) was grown at 600 °C and at a V/III ratio of 55.” should be “...were 600 °C

Figure 1. Published: December 15, 2011 © 2011 American Chemical Society

524

dx.doi.org/10.1021/nl2042886 | Nano Lett. 2012, 12, 524−525

Nano Letters

Addition/Correction

and 55, respectively. WZ nanowire (NW3) was grown at 660 °C and at a V/III ratio of 18.” On page 4315 left-hand column, lines 25−27, “For NW2, Tg is higher than for NW1 and same as for NW3, and V/III ratio is same as that of NW1 and lower than that of NW3.” should be “For NW2, Tg is higher than for NW1 and same as for NW3, and V/III ratio is same as that of NW1 and higher than that of NW3.”