M. Tosaka,* D. Kawakami, K. Senoo, S. Kohjiya, Y. Ikeda, S. Toki, and B. S. Hsiao: Crystallization and Stress Relax-
ation in Highly Stretched Samples of Natural Rubber and Its Synthetic Analogue. Volume 39, Number 15, July 25, 2006, pp 5100-5105. We found that there were mistakes in the experiment and the data processing for the exposure condition 2 of the IR1 sample. Accordingly, Table 2 and Figures 4b and 6b should be replaced by the following items.
Figure 4b.
Figure 6b. Table 2. Exposure Conditions for the WAXD Study
condition
exposure length (s)
cycle length (s)
max value of t (s)
1 2 3
0.036 0.036 0.100
0.083 1 30
8 30 1800
10.1021/MA061798V Published on Web 08/22/2006
applied samples all all except for IR1 NR1, NR4, NR5, NR10, IR2, IR4, IR5